One thing I forgot is the rod quality has a lot to do with the finished product. If the rod you were using wasn't stored correctly in a rod oven, and moisture got to the shield coating, poor or no shielding would be provided. This would cause a lot of globbing and excessive spatter instead of a good concentrated shielded weld puddle...