FEL Bucket weld cracks.

   / FEL Bucket weld cracks. #1  

kensfarm

Veteran Member
Joined
Feb 20, 2003
Messages
1,119
Location
Thurmont, Maryland
Tractor
TC35D w/ SS
I just noticed this the other day.. a series of vertical cracks on each side of the horizontal welds.. on the bottom bucket plate. The cracks are only 1/4 inch.. but I was surprised that all the welds had cracks on each side. I have a NH TC35D w/ SS.. 17LA.. w/ 72inch HD bucket.. almost at 600 hours. I was wondering if anyone else has seen this on their buckets.. I guess if the weld was continous across the bucket.. it might of held up better.
 
   / FEL Bucket weld cracks.
  • Thread Starter
#3  
Yes.. I will take some pictures.. sorry for the delay.. had 65 rolls of fencing delivered on Fri.. each roll weights over 200 lbs.. even w/ the FEL helping me move to store it.. def. a tiring task. After looking at some pictures.. I believe my bucket is not HD.. thought that's what I ordered & payed for.. I'll have to check my order/receipt.. but it's been 3 years.
 
   / FEL Bucket weld cracks. #4  
Guess youve been using the bucket for real. My little B7100 managed to crack frame and bucket welds more than once. Once redone they have held up well. Replacing the worn cutting edge with a much heavier one has also helped.

Egon
 

Tractor & Equipment Auctions

UNUSED FUTURE ML32 - 32" MINI HYD MULCHER (A52706)
UNUSED FUTURE ML32...
2014 Freightliner M2 106 Palfinger PK22002EH Knuckleboom Crane Truck (A55973)
2014 Freightliner...
KOMATSU PC138US-10 EXCAVATOR (A52709)
KOMATSU PC138US-10...
Pnuematic Transfer Pump on Rolling Cart (A59076)
Pnuematic Transfer...
2015 Komatsu WA380-8 Wheel Loader, S/N A74124, PIN# KMTWA130CFNA74124, Diesel Engine, Komatsu WA380 (A59076)
2015 Komatsu...
WHIRLPOOL WASHER & KENMORE ELITE DRYER (A54757)
WHIRLPOOL WASHER &...
 
Top