OK. I hear eveyone on the steel wool. Hired guy just got back with a lifetime supply of #3 steel wool and also some same in stainless steel wool. We were putting it in place with Liquid Nails but /pine's idea on body putty being harder and longer lasting made so much sense I switched.
Now we are using 3M 5200 hardenable Marine Filler - even better than body putty. Comes in a tube and hardens and lasts forever.
Our high tech solution is smearing 5200 into the hole along with steel wool and poking all into place with a whittled down dowel rod.
Thanks,
rScotty
	
		
			
		
		
	
				
			Now we are using 3M 5200 hardenable Marine Filler - even better than body putty. Comes in a tube and hardens and lasts forever.
Our high tech solution is smearing 5200 into the hole along with steel wool and poking all into place with a whittled down dowel rod.
Thanks,
rScotty